Skip to main navigation Skip to search Skip to main content

Modeling of Nanoindentation and Microstructural Ductile Behavior in Metallic Material Systems

  • Jeong B Ma
  • , W Ashmawi
  • , MA Zikry
  • , D Schall
  • , DW Brenner

Research output: Contribution to journalArticle

Original languageEnglish
JournalMRS Online Proceedings Library Archive
Volume841
StatePublished - 2004